Muhrlangantitan mashfiltrlash, skrining va boshqa ilovalarda keng qo'llaniladigan material bo'lib, odatda sof titandan tayyorlanadi. Quyida ba'zi umumiy shtamplangan titanium to'rning texnik xususiyatlari keltirilgan. Haqiqiy texnik xususiyatlar maxsus dastur va ishlab chiqaruvchiga qarab farq qilishi mumkin.
- Material: CP1 kabi sof titan (umumiy sof titaniumlardan biri).
- Qalinligi: Odatda 0,5 mm dan 2 mm gacha, ilova talablariga qarab.
- To'r teshigi o'lchami: Gözenek hajmi filtrlash yoki skrining talablariga qarab farq qilishi mumkin. Umumiy diafragma o'lchamlari 3,5x4 dan 14x40 mm gacha.
- Teshik oralig'i: Teshik qadami qo'shni teshiklarning markazlari orasidagi masofani anglatadi. Bu, shuningdek, maxsus dastur ehtiyojlariga bog'liq va mijozlar talablariga muvofiq sozlanishi mumkin.
- Yuzaki ishlov berish: Ba'zi shtamplangan titan to'rli ekranlar muayyan ishlash talablariga javob berish uchun sirtni tozalashni talab qilishi mumkin, masalan, tuzlash yoki qoplama.
- O'lchovlar: Uzunlik va kenglik o'lchamlari muayyan foydalanish stsenariylari va mijozlar ehtiyojlariga qarab o'zgaradi. Ba'zi ilovalar uchun katta shtamplangan titan to'r kerak bo'lishi mumkin, boshqa ilovalar esa kichikroq o'lchamlarni talab qilishi mumkin.
- Shakl: Shtamplangan titanium to'r kvadrat, to'rtburchaklar, yumaloq va boshqalar kabi ehtiyojlarga ko'ra turli shakllarda tayyorlanishi mumkin.
Hajmi va ruxsat etilgan tolerantligititan to'r varag'i.
| Qalinligi/mm | Qalin bardoshlik | Keng to'r | Keng bag'rikenglik | To'r uzunligi | Uzunlik bardoshliligi |
| >0.5 | ±0.05 | 400~1200 | +15/0 | <=2000 | +20/0 |
| >0.5~0.8 | ±0.07 | ||||
| >0.8~1.1 | ±0.09 | ||||
| >1.1~1.5 | ±0.11 |

| LWM(B) | Tolerantlik | SWD(A) | Tolerantlik | Kesilgan novda (F) | Tolerantlik |
| 4 | ±0.1 | 3.5 | ±0.2 | 0.5 | ±0.2 |
| 6.1 | ±0.15 | 3.7 | ±0.2 | 0.8 | ±0.1 |
| 8 | ±0.15 | 4.5 | ±0.2 | 1.5 | ±0.1 |
| 10 | ±0.15 | 4.5 | ±0.2 | 1.5 | ±0.15 |
| 10 | ±0.15 | 5 | ±0.2 | 1.52 | ±0.15 |
| 10.3 | ±0.15 | 6 | ±0.2 | 1.5 | ±0.15 |
| 12.5 | ±0.15 | 4.5~6.5 | ±0.2 | 1.7 | ±0.2 |
| 12.5 | ±0.15 | 5.6 | ±0.2 | 1.8 | ±0.2 |
| 13 | ±0.15 | 5.5 | ±0.2 | 1.5 | ±0.2 |
| 13 | ±0.15 | 5.8 | ±0.2 | 1.9 | ±0.2 |
| 20 | ±0.20 | 7 | ±0.2 | 1.7 | ±0.2 |
| 40 | ±0.20 | 14 | ±0.2 | 1.7 | ±0.2 |

Titan to'r qancha turadi?
Titan to'rning narxi bir necha omillarga, jumladan titanium darajasiga, to'rning qalinligi va o'lchamlariga va etkazib beruvchiga qarab farq qilishi mumkin. Titan odatda qimmat materialdir va uning narxi bozor sharoitlari va mavjudligiga qarab o'zgarishi mumkin.
Titan to'rning narxi ishlab chiqarish va qayta ishlash xarajatlarini ham o'z ichiga oladi, bu esa yakuniy narxga yanada ta'sir qilishi mumkin; Titan to'r narxini hozir biz bilan bog'laningsales@tmsalloy.com.