Titanium alloy can not only make marine equipment develop towards "deep, large, far, high ", but also fully realize the same life as the main body of marine equipment. It is the best choice for marine equipment. At present, China pays more attention to the application of titanium in marine equipment, and the amount of titanium used is also increasing. Deep-sea pressure shell, seawater pipeline, cylinder superstructure, frame, etc. will become the key development direction of marine titanium.

Hozirgi vaqtda yuk tashish sanoatida titanning ko'plab ilovalari uyda va chet elda mavjud.
However, the material system in relevant specifications is not perfect. It is hoped that relevant units will organize discussion and improve the material system in current relevant codes such as Titanium Pressure Vessel, Material and Welding, so as to facilitate the designer's reference.
Upper buildings:
Hozirgi vaqtda ichki harbiy kemaning yuqori tuzilishida ba'zi qo'llash misollari mavjud, masalan, mast uchun Ti70 (TA23), radar antennasi uchun TA5 va TA7 bar, angar terisi uchun TA2 va TA5 plitalari va ramka tuzilishi.
Titan, shuningdek, LPD17 amfibiya dock transport kemasining yuqori binolarida keng qo'llaniladi, bu uning massasini taxminan 50 foizga kamaytiradi va barqarorligini sezilarli darajada yaxshilaydi.
Boshqa sohalarda ishlab chiqarish ilovalari
Yuqoridagi bosimga chidamli korpus, quvurlar tizimi va ustki tuzilmalarda ishlatiladigan katta miqdorda titandan tashqari, boshqa komponentlar ham uyda va xorijda dengiz uskunalarida foydalidir.