1. Tantal plitasiR05200 sof tantal va tantal qotishmasidan tayyorlangan yupqa metall qatlam bo'lib, u nodir refrakter metall bo'lgan Ta varaq yoki plastinka deb ham ataladi.
2. R05200 Tantal varag'i mavjud o'lcham va nav
Darajasi: Ta1 R05200 Ta2 R05400
Standart: ASTM B 708
Soflik: 99,95 foiz 99,99 foiz
Yuzaki: rangli metall rang
Zichlik: 16,5 g/sm3
Erish nuqtasi: 2980 daraja


3. Kimyoviy tarkibi
| Kimyoviy tarkibi, Maks | |||||||||||
| Baho | C | N | O | H | Fe | Si | Ti | Ni | Nb | W | Mo |
| Ta1 | 0.004 | 0.005 | 0.02 | 0.002 | 0.005 | 0.005 | 0.002 | 0.005 | 0.05 | 0.002 | 0.002 |
4. Tantal lavhaning mexanik xususiyatlari
| Baho | Davlat | Qalinligi (mm) | Kuchlanish kuchi (MPa) | Cho'zilish (foiz) |
| Ta1 | M | 0.1~0.5 | 207 dan katta yoki unga teng | 25 dan katta yoki teng |
| >0.5~3.0 | 30 dan katta yoki teng |
5. R05200 tantal varaqining ilovalari qanday?
R05200 tantal plitasi isitish qismlari, issiqlik izolyatsion qismlari va vakuumli portlash pechlari uchun zaryadlovchi idishlarni tayyorlash uchun ishlatiladi. U kimyo sanoatida parchalanuvchilar, isitgichlar, sovutgichlar, turli xil idishlar va asboblarni tayyorlash uchun ishlatilishi mumkin, shuningdek, aviatsiya, aerokosmik sanoat, tibbiy asboblar va boshqa sohalarda keng qo'llanilishi mumkin.
6. Tantal lavhaning diametri va bardoshliligi qanday?
| Qalinligi | Tolerantlik | Kengligi | W bag'rikenglik | Uzunlik | L bag'rikenglik | |
| I daraja | II daraja | |||||
| 0.15~0.2 | ±0.015 | ±0.02 | 50-300 | ±2.0 | 100-1000 | ±2.0 |
| >0.2~0.3 | ±0.020 | ±0.03 | 50-300 | ±2.0 | 100-1000 | ±2.0 |
| >0.3~0.5 | ±0.030 | ±0.04 | 50-300 | ±2.0 | 100-1000 | ±2.0 |
| >0.5~0.8 | ±0.040 | ±0.06 | 50-200 | ±1.0 | 50-700 | ±2.0 |
| >0.8~1.0 | ±0.060 | ±0.08 | 50-200 | ±1.0 | 50-700 | ±2.0 |
| >1.0~1.5 | ±0.080 | ±0.10 | 50-200 | ±1.0 | 50-700 | ±2.0 |
| >1.5~2.0 | ±0.120 | ±0.14 | 50-200 | ±1.0 | 50-700 | ±2.0 |
| >2.0~3.0 | ±0.160 | ±0.18 | 50-200 | ±1.0 | 50-700 | ±2.0 |
| >3.0~4.0 | ±0.180 | ±0.20 | 50-200 | ±1.0 | 50-700 | ±1.0 |
| >4.0~6.0 | ±0.200 | ±0.24 | 50-200 | ±1.0 | 50-700 | ±1.0 |
7. ning afzalliklaritantal lavha metall
Tantal metall qatlami kislotalar, ishqorlar, tuzlar va organik muhitlarga nisbatan yaxshi kimyoviy barqarorlikka ega, faqat platina va oltindan keyin ikkinchi o'rinda turadi. Ftor, gidroflorik kislota va ftorid ionlari, dumanli nitrat kislota va sulfat kislota o'z ichiga olgan kislotali eritmalardan tashqari, ko'pgina muhitlarda tantal korroziyaga uchramaydi.
8. Qayerdan sotib olish keraktantal plitasi?
Etakchi noyob o'tga chidamli metall tantal plitasi yetkazib beruvchilaridan biri sifatida biz ko'p yillik metallni qayta ishlash tajribasiga egamiz, biz mijozlarga barqaror sifatli mahsulotlarni taqdim etmaymiz, shuningdek, R05200 Tantal varaqini sotib olishni istasangiz, biz bilan bog'laning. da sales@tmsalloy.com

Issiq teglar: tantal plitasi, etkazib beruvchilar, ishlab chiqaruvchilar, zavod, narx, ommaviy, sotuvda, stokda, chegirma sotib oling