1. Gr1 titanium bar 99,5 foiz titandan yasalgan mustahkam bar, kumush-oq yorqin sirtga ega.

2. Asosiy ma'lumotlar

Titan bar shakli: yumaloq, kvadrat va to'rtburchaklar

Olchamlari: buyurtma asosida tayyorlangan o'lcham mavjud

Titan novda ishlab chiqarish holati:

Issiq ishlov berish holati (R)

Sovuq ish holati (Y)

Yuvish holati (M)

3. ASTMB348 bo'yicha Gr1 titanium barning kimyoviy va mexanik xususiyatlari

kimyoviy elementlarNCH FeO Har birining maksimal qoldiqlariMaksimal qoldiqlar
1-sinf0.030.080.0150.20.180.10.4
Bahokuchlanish kuchi MpaOqim kuchi Mpacho'zilish
1-sinf24013824

4. Titan novda qo'llanilishi:

Biz turli sohalar uchun titanium novdalarni taqdim etamiz. Ushbu materialning eng keng tarqalgan qo'llanilishi aviatsiya, neft-kimyo sanoati, suv tozalash inshootlarini qurish, elektr energiyasini ishlab chiqarish inshootlari va dengiz transporti vositalarini o'z ichiga oladi.

Tafsilotlar namoyishi


titanium rod

Gr1 titanium bar

6mm titanium rod

titaniumli dumaloq bar

5. Titan barlar uchun ruxsat etilgan bardoshlik - issiq haddelenmiş dumaloq va kvadrat barlar

Belgilangan o'lcham, dyuym (mm)O'lchamdagi o'zgarishlar,
dyuym (mm)
Davradan tashqari A yoki Kvadratdan tashqari, B dyuym (mm)
1 ⁄ 4 dan 5 ⁄ 16 (6,35 dan 7,94 gacha), shu jumladan±0.005 (0.13) 0.008 (0.20)
5 ⁄ 16 dan 7 ⁄ 16 (7,94 dan 11,11 gacha), shu jumladan±0.006 (0.15) 0.009 (0.23)
7 ⁄ 16 dan 5 ⁄ 8 (11,11 dan 15,88 gacha), shu jumladan±0.007 (0.18) 0.010 (0.25)
5 ⁄ 8 dan 7 ⁄ 8 (15,88 dan 22,22 gacha), shu jumladan±.008 (0.20) 0.012 (0.30)
7 ⁄ 8 dan 1 gacha (22,22 dan 25,40 gacha), shu jumladan±0.009 (0.23) 0.013 (0.33)
1 dan 1 1 ⁄ 8 gacha (25,40 dan 28,58 gacha), shu jumladan±0.010 (0.25) 0.015 (0.38)
1 1 ⁄ 8 dan 1 1 ⁄ 4 gacha (28,58 dan 31,75 gacha), shu jumladan±0.011 (0.28) 0.016 (0.41)
1 1 ⁄ 4 dan 1 3 ⁄ 8 gacha (31,75 dan 34,92 gacha), shu jumladan ±0.012 (0.30) 0.018 (0.46)
1 3 ⁄ 8 dan 1 1 ⁄ 2 gacha (34,92 dan 38,10 gacha), shu jumladan ±0.014 (0.36) 0.021 (0.53)
1 1 ⁄ 2 dan 2 gacha (38,10 dan 50,80 gacha), shu jumladan ± 6 1 ⁄ 64 (0.40) 0.023 (0.58)
2 dan 2 1 ⁄ 2 gacha (50,80 dan 63,50 gacha), shu jumladanortiqcha 1 ⁄ 32 , − 0 (0,79)0.023 (0.58)
2 1 ⁄ 2 dan 3 1 ⁄ 2 gacha (63,50 dan 88,90 gacha), shu jumladanortiqcha 3 ⁄ 64 , − 0 (1,19)0.035 (0.89)
3 1 ⁄ 2 dan 4 1 ⁄ 2 gacha (88,90 dan 114,30 gacha), shu jumladanortiqcha 1 ⁄ 16 , − 0 (1,59)0.046 (1.17)