Titan yong'oqlari

Titan yong'oqlari

Titan yong'oqlari va yuvish vositalari
Titan gardishli yong'oq
So'rov yuborish
Hozir chat
Ta'rif

 

Mahsulotlar bilan tanishtirish

1. Titan yong'oqlari - mahkamlash uchun murvat yoki vintlar bilan vidalanadigan qismlar. Turli materiallarga ko'ra, u karbonli po'lat, zanglamaydigan po'lat, titanium va boshqa asosiy turlarga bo'linadi.

2. Asosiy ma'lumotlar

2 va 5 darajalar titan vintlardek eng ko'p ishlatiladigan navlardir:

• 2-darajali (UNS R50400 / 3.7035): Savdo uchun sof titan va eng keng tarqalgan vintli nav.

• 5-darajali (UNS R56400 / 3.7165): Ajoyib kuch va vazn nisbati, korroziyaga chidamlilik va yuqori quvvatning noyob kombinatsiyasiga erishadi.

Standartlar: DIN934, ISO, BS, JIS

Turi: titaniumli gardish yong'oqlari, titaniumli to'liq yong'oqlar, titaniumli neylon yong'oqlar, titaniumli olti burchakli yong'oqlar, titaniumli gaykalar, titaniumli gardishli metall gaykalar.

3. Titan biriktirgichlar mustahkamligi, yengilligi va korroziyaga chidamliligi bilan mashhur. Ular xlor-ishqor, dengiz, dengiz neft va gaz, tuzni tozalash, tibbiyot va sellyuloza-qog'oz kabi ko'plab sohalar uchun zarurdir.

Tafsilotlar namoyishi

titanium nuts

Titan yong'oqlari

Titanium Flanged Nut

Titan gardishli yong'oq

4. DIN934 bo'yicha titan yong'oqlari o'lchami

Ip hajmi
d
M1M1.2M1.4M1.6(M1.7)M2(M2.3)M2.5(M2.6)M3(M3.5)M4M5M6(M7)M8
















PPitchDag'al ip0.250.250.30.350.350.40.450.450.450.50.60.70.8111.25
Nozik ip///////////////1
Nozik ip////////////////
mmaksimal=nominal oʻlcham
min

0.811.21.31.41.61.8222.42.83.2455.56.5

0.550.750.951.051.151.351.551.751.752.152.552.93.74.75.26.14
mwmin
0.440.60.760.840.921.081.241.41.41.722.042.322.963.764.164.91
smaksimal=nominal oʻlcham
min

2.5333.23.544.5555.5678101113

2.42.92.93.023.383.824.324.824.825.325.826.787.789.7810.7312.73
e ①min
*

2.713.283.283.413.824.324.885.455.456.016.587.668.7911.0512.1214.38

----------------
1000 birlik uchun ≈ kg
0.030.0540.0630.0760.10.1420.20.280.720.3840.5140.811.232.53.125.2
Ip hajmi
d
M10M12(M14)M16(M18)M20(M22)M24(M27)M30(M33)M36(M39)M42(M45)M48
















PPitchDag'al ip1.51.75222.52.52.5333.53.5444.54.55
Nozik ip11.51.51.51.521.5222233333
Nozik ip1.251.25//21.52/////////
mmaksimal=nominal oʻlcham
min

8101113151618192224262931343638

7.649.6410.312.314.314.916.917.720.722.724.727.429.432.434.436.4
mwmin
6.117.718.249.8411.4411.9213.5214.1616.5618.1619.7621.9223.5225.927.529.1
smaksimal=nominal oʻlcham
min

17192224273032364146505560657075


16.7318.6721.6723.6726.1629.16313540454953.858.863.168.173.1
e ①min
*

18.921.124.4926.7529.5632.9535.0339.5545.250.8555.3760.7966.4471.376.9582.6

----------------
1000 birlik uchun ≈ kg11.617.32533.349.464.479110165223288393502652800977
Ip hajmi
d
(M52)M56(M60)M64(M68)M72(M76)M80(M85)M90M100M110M125M140M160
















PPitchDag'al ip55.55.566//////////
Nozik ip3444/6666666666
Nozik ip////444444444//
mmaksimal=nominal oʻlcham
min

424548515458616468728088100112128

40.443.446.449.152.156.159.162.166.170.178.185.897.8109.8125.5
mwmin
32.334.737.139.341.744.947.349.752.956.162.568.678.287.8100
smaksimal=nominal oʻlcham
min

80859095100105110115120130145155180200230

78.182.887.892.897.8102.8107.8112.8117.8127.5142.5152.5177.5195.4225.4
e ①min
*

88.2593.5699.21104.86110.51116.16121.81127.46133.11144.08161.02172.32200.57220.8254.7

-----------170196216248
1000 birlik uchun ≈ kg122014201690198023002670304034403930493068208200130001750026500

Issiq teglar: titan yong'oqlari, etkazib beruvchilar, ishlab chiqaruvchilar, zavod, narx, ommaviy, sotuvda, stokda, chegirma sotib oling

So'rov yuborish

(0/10)

clearall